Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Azdel
Trade Name Plus
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AZDEL® U400-B01N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This material allows highly directionalized reinforcement where loads are in defined planes.Typically it is combined with Azdel chopped and random mat to localized high stress paths, minimizing part weight and cost. For use in semi-structural applications and especially suited to adhesion bonded assemblies.Commercially available only to European based customers.Information provided by Azdel.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Filler Content 41.5 %
41.5 %
ISO 1172
Thickness 3200 microns
126 mil
AZDEL Test
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
flat plaques, 320 x 320 mm; ISO 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
measured on flat plaques, 320 x 320 mm; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
Transverse direction; ISO 527/4
250 MPa
36300 psi
Longitudinal direction; ISO 527/4
Elongation at Break 2.0 %
2.0 %
Transverse direction; ISO 527/4
2.3 %
2.3 %
Longitudinal direction; ISO 527/4
Tensile Modulus 5.80 GPa
841 ksi
Transverse direction; ISO 527/4
9.30 GPa
1350 ksi
Longitudinal direction; ISO 527/4
Flexural Strength 130 MPa
18900 psi
Transverse direction; ISO 178
250 MPa
36300 psi
Longitudinal direction; ISO 178
Flexural Modulus 5.50 GPa
798 ksi
Transverse direction; ISO 178
8.00 GPa
1160 ksi
Longitudinal direction; ISO 178
Charpy Impact, Notched 6.50 J/cm²
30.9 ft-lb/in²
Transverse direction; ISO 179/2fn
14.0 J/cm²
66.6 ft-lb/in²
Longitudinal direction; ISO 179/2fn