Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall Suprel® 9422 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name Suprel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall Suprel® 9422 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with specifications frequently referenced in the telecommunications industry.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D-638
Tensile Modulus 1.65 GPa
240 ksi
ASTM D-638
Flexural Strength 46.9 MPa
6800 psi
ASTM D-790
Flexural Modulus 1.52 GPa
220 ksi
ASTM D-790
Izod Impact, Notched 2.67 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
5.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
5.71 J/cm

@Thickness 3.17 mm,
Temperature -28.9 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature -20.0 °F
ASTM D-256
8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.00 °C
165.2 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
annealed; ASTM D-648
Flammability, UL94 V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
5VA

@Thickness 2.00 mm
5VA

@Thickness 0.0787 in
Descriptive Properties Value Comments
UL Weatherability Rating F(2)
UL-746C
Copyright © lookpolymers.com All Rights Reserved