Axiall HR-5009 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall HR-5009 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which includes color hold, regrind stability and surface appearance. HR-5009 is NSF listed under standard 14/61 for both potable water and DWV applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D-785
Tensile Strength, Yield 50.3 MPa
7300 psi
ASTM D-638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D-790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
0.700 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
0.587 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 123 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 71.00 °C
159.8 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Oxygen Index 38 %
38 %
ASTM D-2863
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 12454-B
NSF std. 14
Flow Ratio (Distance/Wall Thickness, 390-400°F) 170
Georgia Gulf Test