Axiall EX 3114B Plenum Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall EX 3114B Plenum Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-lead stabilized CAT 3 jacket recommended for hybrid constructions. Also recommended for 25+ pair counts.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.73 - 1.77 g/cc
1.73 - 1.77 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 39 - 45
39 - 45
delayed; ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 220 %
220 %
ASTM D-638
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -8.00 °C
17.6 °F
ASTM D-746
Oxygen Index 44 %
44 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F