Axiall 8941 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8941 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A clear extrusion and molding grade compound with good toughness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.28 g/cc
1.24 - 1.28 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 97
91 - 97
delayed; ASTM D-2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Elongation at Yield 325 %
325 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F