Axiall 8823 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8823 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A UL certified flame retardant, clear flexible PVC compound recommended for a maximum service temperature of 60°C. Exhibits good migration resistance properties. UL approved for 94 V-0 at 2.30 mm; 94 V-1 at 1.85 mm and 94 V-2 at 0.90 mm.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.26 g/cc
1.22 - 1.26 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 86
80 - 86
delayed; ASTM D-2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D-638
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 0.900 mm
V-2

@Thickness 0.0354 in
V-1

@Thickness 1.85 mm
V-1

@Thickness 0.0728 in
V-0

@Thickness 2.30 mm
V-0

@Thickness 0.0906 in
Processing Properties Metric English Comments
Melt Temperature 171 °C
340 °F