Axiall 8710 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8710 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips and flexible gaskets. Excellent for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 74
68 - 74
delayed; ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
100% Modulus 0.00500 GPa
0.725 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 174 °C
345 °F