Axiall 8540 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8540 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.19 - 1.23 g/cc
1.19 - 1.23 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 51 - 57
51 - 57
delayed; ASTM D-2240
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 163 °C
325 °F