Material Notes:
Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such as transparent panels, glazing and protected jalousie windows. It is also suitable for high impact vacuum formed sheet applications, as well as the clear edge on decorator vertical blinds.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D-638
Flexural Strength 84.1 MPa
12200 psi
ASTM D-790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D-790
Izod Impact, Notched 6.67 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 210 kJ/m²
100 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 62.2 °C
144 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.040 inch(min. thickness)
Optical Properties Metric English Comments
Haze 10 %

@Thickness 3.17 mm
10 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 87 %

@Thickness 3.17 mm
87 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F
Descriptive Properties Value Comments
Cell Classification 14442113
ASTM D-4216