Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 7810 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7810 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
105°C rated injection molding compound approved for 94 V-0 in black and white at 0.75 mm and also approved for 94 V-0 in all colors at 1.5 mm.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 84
78 - 84
delayed; ASTM D-2240
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D-638
Elongation at Yield 275 %
275 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
All colors
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
Black & White
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F
Copyright © lookpolymers.com All Rights Reserved