Axiall 7777 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7777 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D-638
Tensile Modulus 3.50 GPa
507 ksi
ASTM D-638
Flexural Strength 80.7 MPa
11700 psi
ASTM D-790
Flexural Modulus 2.43 GPa
352 ksi
ASTM D-790
Izod Impact, Notched 1.98 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.70 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F