Axiall 6741 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 6741 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A low gravity profile extrusion compound recommended for weatherstrips, extruded shapes, hoses and flexible gaskets. Provides good adhesion to rigid PVC in co-extruded products.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.28 - 1.32 g/cc
1.28 - 1.32 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 69 - 75
69 - 75
delayed; ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 425 %
425 %
ASTM D-638
100% Modulus 0.00483 GPa
0.700 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Copyright © lookpolymers.com All Rights Reserved