Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 6651 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 6651 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A clear molding and extrusion compound with good processing characteristics and good low temperature properties. Formulated to be resistant to fungal and microbial attack.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.22 g/cc
1.18 - 1.22 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 69
63 - 69
delayed; ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F
Copyright © lookpolymers.com All Rights Reserved