Material Notes:
Georgia Gulf 6316 is an economical high flow rigid PVC fittings compound designed for drain, waste and vent applications, where higher impact properties are desired. This compound is characterized by excellent processability, which includes color hold, regrind stability, and surface appearance. 6316 is NSF listed under Standard 14, ASTM D-4396 for DWV applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Tensile Strength, Yield 47.4 MPa
6880 psi
ASTM D-638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D-790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 190
Georgia Gulf Test