Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 5009 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 5009 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is required. It has full NSF approval and is suitable for all types of water distribution systems, including pressure fittings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D-785
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D-638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D-790
Izod Impact, Notched 0.320 J/cm

@Thickness 6.35 mm,
Temperature -20.0 °C
0.600 ft-lb/in

@Thickness 0.250 in,
Temperature -4.00 °F
ASTM D-256
0.427 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.800 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 123 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.00 °C
165.2 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Oxygen Index 38 %
38 %
ASTM D-2863
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 12454-B
NSF std. 14
Flow Ratio (Distance/Wall Thickness, 390°F) 130
Georgia Gulf Test