Axiall 47551 Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 47551 Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.25 - 1.29 g/cc
1.25 - 1.29 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 71 - 77
71 - 77
delayed; ASTM D-2240
78 - 84
78 - 84
ASTM D-2240
Tensile Strength, Yield 14.5 MPa
2100 psi
ASTM D-638
Elongation at Yield 330 %
330 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 149 °C
300 °F