Material Notes:
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Elongation at Yield 250 %
250 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 149 °C
300 °F