Axiall 22930 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 22930 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Jacket compound suitable for riser applications when used with flame retardant PVC primaries. Maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.43 g/cc
1.39 - 1.43 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 96
90 - 96
delayed; ASTM D-2240
Tensile Strength, Yield 19.0 MPa
2750 psi
ASTM D-638
Elongation at Yield 300 %
300 %
ASTM D-638
100% Modulus 0.0138 GPa
2.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D-746
Oxygen Index 32.5 %
32.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F