Material Notes:
Non-lead stabilized, 75C rated jacketing compound suitable for CATV, CM, CL2 type applications. UL recognized for 94 V-0 in all colors at 1.5 mm. QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.39 g/cc
1.35 - 1.39 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 86
80 - 86
delayed; ASTM D-2240
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Elongation at Yield 273.6 %
273.6 %
Air Aging: 10 days @ 100°C; 30 mil slabs; UL 1581
320 %
320 %
ASTM D-638
100% Modulus 0.0103 GPa
1.50 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D-746
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
All colors
Oxygen Index 30 %
30 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F