Axiall 2134N Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 2134N Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness) and 94 V-0 in black and white (1.5 mm min. thickness). UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D-638
Elongation at Yield 335 %
335 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D-746
Flammability, UL94 V-2

@Thickness >=0.750 mm
V-2

@Thickness >=0.0295 in
All colors
V-0

@Thickness >=1.50 mm
V-0

@Thickness >=0.0591 in
Black & White
Oxygen Index 25 %
25 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F