Axiall 19730 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 19730 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrical grade 105°C rated vinyl elastomer compound suitable for SEO and SJEO insulation and jacket applications per UL 62.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.33 g/cc
1.29 - 1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 76
70 - 76
delayed; ASTM D-2240
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D-638
Elongation at Yield 326.3 %
326.3 %
Oil Aging: 168 hours @ 60°C; #2 Oil; UL 1581
332.3 %
332.3 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
375 %
375 %
ASTM D-638
100% Modulus 0.00610 GPa
0.885 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -38.0 °C
-36.4 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+12 ohm-cm
6.00e+12 ohm-cm
50% RH; ASTM D-257
Dielectric Constant 5.53

@Frequency 1000 Hz
5.53

@Frequency 1000 Hz
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F
Users viewing this material also viewed the following: