Material Notes:
105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistant applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 42 - 48
42 - 48
delayed; ASTM D-2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Elongation at Yield 293 %
293 %
Air Aging: 168 hours @ 113°C; 30 mil slabs; UL 1581
303.6 %
303.6 %
Oil Aging: 96 hours @ 100°C; 30 mil slabs; UL 1581
330 %
330 %
ASTM D-638
100% Modulus 0.0159 GPa
2.30 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -10.0 °C
14.0 °F
ASTM D-746
Oxygen Index 25.5 %
25.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F