Material Notes:
60C plug molding component. UL recognized component for 94 V-0 in all colors. 1.13 mm minimum thickness. UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.48 - 1.52 g/cc
1.48 - 1.52 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93
87 - 93
delayed; ASTM D-2240
Tensile Strength, Yield 15.9 MPa
2300 psi
ASTM D-638
Elongation at Yield 265 %
265 %
ASTM D-638
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D-638
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness >=1.13 mm
V-0

@Thickness >=0.0445 in
All colors
Oxygen Index 29.5 %
29.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F