Axiall 18752 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 18752 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrical grade extrusion compound with excellent low temperature performance. Maximum service temperature of 105°CInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78
72 - 78
delayed; ASTM D-2240
Tensile Strength, Yield 13.1 MPa
1900 psi
ASTM D-638
Elongation at Yield 280 %
280 %
Air Aging: 168 hours @ 136°C; 70 mil slabs; UL 1581
320.3 %
320.3 %
Oil Aging: 4 hour @ 80°C; #2 Oil; 35 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F