Axiall 1275 Plenum Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 1275 Plenum Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plenum-grade optical fiber jacket. UL QMTM2 recognized component for plenum cable compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.61 - 1.65 g/cc
1.61 - 1.65 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 56
50 - 56
delayed; ASTM D-2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D-638
Elongation at Yield 128 %
128 %
Air Aging: 7 days @ 100°C; UL 1581
160 %
160 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -5.00 °C
23.0 °F
ASTM D-746
Oxygen Index 42 %
42 %
ASTM D-638
Electrical Properties Metric English Comments
Dielectric Constant 4.59

@Frequency 1e+6 Hz
4.59

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F