Material Notes:
AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. AA-SUPERTHERM 05 bonds readily to itself, and to metals, silica, alumina, sapphire and other ceramics, glass, plastics and many other materials, because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fully cured AA-SUPERTHERM 05 provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils, and alcohol. AA-SUPERTHERM 05 passes NASA`s outgassing specification making it ideal for demanding space applications. Appearance: WhiteCure Type: Heat cure or Room TemperatureBenefits:StrongDurableHigh-impact bondsFullycuredExcellent resistance to many chemicals Mix Ratio by weight: 100:100/Resin:HardenerSubstrates: metals, silica, alumina, sapphire and other ceramics, glass, plastics and many other materials Typical Application: Extremely sensitive thermal cooling applicationsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.30 g/cc
2.30 g/cc
mixed, uncured
Viscosity 33000 cP
33000 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Izod Impact, Notched 0.262 J/cm
0.490 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 25.9 µm/m-°C
14.4 µin/in-°F
Thermal Conductivity 1.06 W/m-K
7.36 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 48.0 °C
118 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.20e+13 ohm-cm

@Temperature 75.0 °C
3.20e+13 ohm-cm

@Temperature 167 °F
2.10e+15 ohm-cm

@Temperature 25.0 °C
2.10e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 5.9

@Frequency 1000 Hz
5.9

@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm
410 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 45.0 min
45.0 min
uncured