Material Notes:
AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, and superior mechanical properties are required.Appearance: AmberCure Type: Heat cure or Room TemperatureBenefits:High fillEasy handlingGood wettingToughnessHigh TempFast cureLow Viscosity Substrates: Most material surfaces, including many metals, rigid plastics, glass, ceramics, leather, rubber, wood and concrete Typical Application: Industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, and superior mechanical properties are required.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
mixed, uncured
Viscosity 600 cP
600 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Tensile Strength, Yield 37.2 MPa
5400 psi
Elongation at Yield 10 %
10 %
Shear Strength 17.2 MPa
2500 psi
Lap, Alum to Alum
Thermal Properties Metric English Comments
CTE, linear 64.1 µm/m-°C
35.6 µin/in-°F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 70.0 °C
158 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+14 ohm-cm
1.20e+14 ohm-cm
Dielectric Constant 3.35

@Frequency 1000 Hz
3.35

@Frequency 1000 Hz
Dielectric Strength 18.1 kV/mm
460 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 75.0 min
75.0 min
uncured