Atom Adhesives AA-BOND F156 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND F156 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND F156 is a black, solvent free thixotropic epoxy recommended for high quality photographic industry, laminating, production and repair applications where a room temperature cure optically opaque adhesive for light sensitive components is required. AA-BOND F156 is two parts smooth paste formulation is easy to use, develops strong bonds to itself and to most materials. AA-BOND F156 exhibits low shrinkage during cure, has excellent dimensional stability over a wide temperature range.Appearance: Black, Opaque Cure Type: Heat cure or Room TemperatureBenefits:Easy to useGood low-temperature structural, physical and electrical propertiesIt’s resistant to water, weater, gases, salts, mild acids, alkalis, and many organic and inorganic compounds Mix Ratio by weight: 100:12/Resin:Hardener Substrates: Glass and glass fabrics, ceramics, leather, metals and many plastics Typical Application: High quality photographic industry bonding, laminating, production and repair applications where a room-temperature cure optically opaque adhesive for light sensitive components is requiredInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Viscosity 50000 cP
50000 cP
After mixing, uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
cured
Thermal Properties Metric English Comments
CTE, linear 32.9 µm/m-°C
18.3 µin/in-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 95.0 °C
203 °F
cured
Electrical Properties Metric English Comments
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 15.4 kV/mm
390 kV/in
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min