Material Notes:
AA-BOND F112 is an impact resistant, fiber-optic adhesive. AA-BOND F112 is two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. AA-BOND F112 allows more connectors to be produced from one mix. Low stress, AA-BOND F112 is an excellent choice for multimode connectors and single mode connectors where excessive curing temperatures may cause cracking. AA-BOND F112 can be cured at room temperature overnight or as fast as 15 minutes at 90°C. The blue color facilitates easy polishing and its cured properties prevent pistoning. This product is a 100% solid system that can be used for small potting and sealing applications where resistance to thermal shock and impact are required.Appearance: Dark BlueCure Type: Heat cure or Room TemperatureBenefits:Low viscosityThermal shock and impact resistant Mix Ratio by weight: 100:30/Resin:Hardener Typical Application: Fiber optic assembly, multimode and single mode connectors, small potting and sealing applicationsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
uncured
Water Absorption 0.070 %
0.070 %
Viscosity 1800 cP
1800 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Shear Strength 17.2 MPa

@Temperature 25.0 °C,
Time 86400 sec
2500 psi

@Temperature 77.0 °F,
Time 24.0 hour
Lap, Alum to Alum
20.7 MPa

@Temperature 65.0 °C,
Time 3600 sec
3000 psi

@Temperature 149 °F,
Time 1.00 hour
Lap, Alum to Alum
29.6 MPa

@Temperature 90.0 °C,
Time 900 sec
4300 psi

@Temperature 194 °F,
Time 0.250 hour
Lap, Alum to Alum
Thermal Properties Metric English Comments
CTE, linear 61.9 µm/m-°C
34.4 µin/in-°F
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 102 °C
216 °F
Optical Properties Metric English Comments
Refractive Index 1.51
1.51
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 90.0 °C
0.250 hour

@Temperature 194 °F
60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min
uncured
Descriptive Properties Value Comments
Thixotropic Index 1