Material Notes:
AA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronics, aerospace, and industrial applications where a high-fill, non-sag reliable adhesive is required for bonding and enhancing the mechanical and structural rigidity of assemblies. AA-BOND 2116 is two-part, solvent-free compound is readily mixed, handled, used, and cured at room temperature, and develops strong bonds to most clean, dry material surfaces including metals, glass, ceramics, wood and many plastics. AA-BOND 2116 bonds provide electrical insulation and excellent resistance to weather, galvanic action, petroleum solvents and lubricants, gasoline, jet fuels, alcohol, salts, and mild acids and alkalis.Appearance: Milky, transparentCure Type: Heat cure or Room TemperatureBenefits:Passes NASA’s Outgassing/Low OutgassingSolvent freeWeather resistant Mix Ratio by weight: 100:22/Resin:HardenerSubstrates: Ceramics, glass to glass, fabrics, metals, laminates and other composite materialsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
Solids Content 100 %
100 %
reactive, uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
Thermal Properties Metric English Comments
CTE, linear 55.1 µm/m-°C
30.6 µin/in-°F
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm
1.00e+10 ohm-cm

@Temperature 100 °C
1.00e+10 ohm-cm

@Temperature 212 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min