Material Notes:
Stainless mould steel with a unique combination of toughness, corrosion resistance and through-hardening properties.Applications: For all type of moulds, especially suited for larger tools where corrosion in production is unacceptable and where high surface finish is requiredAISI 420 mod
Mechanical Properties Metric English Comments
Hardness, Brinell 250
250
hardness supplied.