Assab Steels ELMAX Plastic Mold Material

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Assab Steels
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Assab Steels ELMAX Plastic Mold Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Powder tool steel. Stainless plastic mould steel with high wear resistance.Applications: Electronics industry: connectors, plugs, switches, resistors, integrated circuits. Food processing industry: corrosion resistance and wear resistance.
Mechanical Properties Metric English Comments
Hardness, Brinell 240
240
hardness supplied.
Component Elements Properties Metric English Comments
Carbon, C 1.7 %
1.7 %
Chromium, Cr 18 %
18 %
Iron, Fe 76 %
76 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 1.0 %
1.0 %
Vanadium, V 3.0 %
3.0 %