Assab Steels 707 Machinery Steel

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Assab Steels
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Assab Steels 707 Machinery Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloyed machinery steel suitable for weldingApplications: Used for shafts, gears, sprockets, etc., particularly when weldability is required.AISI 4130, W.nr 1.7218, JIS SCM2
Mechanical Properties Metric English Comments
Hardness, Brinell 215 - 260
215 - 260
Hardness supplied approx.
Component Elements Properties Metric English Comments
Carbon, C 0.25 %
0.25 %
Chromium, Cr 1.05 %
1.05 %
Iron, Fe 97.75 %
97.75 %
Manganese, Mn 0.75 %
0.75 %
Molybdenum, Mo 0.20 %
0.20 %