Asia Technology Pioneers CAP 702 PP Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Asia Technology Pioneers
Trade Name CAP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asia Technology Pioneers CAP 702 PP Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAP702 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood dimensional (Heat) stabilityOutstanding surface appearanceUV resistance Hi Scratch resistanceCertification:ISO 9001:2008Iranian Nano Technology Initiative Council CertificationCertification from automakersApplication:Automotive Dashboard Frame and ConsoleInformation provided by Asia Technology Pioneers
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Melt Flow 13 g/10 min

@Temperature 230 °C
13 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 21.6 MPa
3130 psi
ASTM D638M
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm
2.20 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Form Pellets - Gray color
Processing Method Injection Molding
Reinforcement Additives Nano Particles