Ashley Polymers Ashlene® RH190TB Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® RH190TB Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity, black.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648