Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® RH190ST Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® RH190ST Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high impact homopolymer resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Moisture Absorption at Equilibrium 0.28 %
0.28 %
50% RH; ASTM D570
Melt Flow 6.0 g/10 min
6.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648