Material Notes:
A 20% PTFE filled Acetal for outstanding wear characteristics and low friction.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Water Absorption 0.18 %
0.18 %
ASTM D570
Melt Flow 6.0 g/10 min
6.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 166 °C
331 °F
ASTM D648