Ashley Polymers Ashlene® PB1410 Polycarbonate, 10% Glass Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® PB1410 Polycarbonate, 10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 10% glass reinforced polycarbonate for increased mechanical strength and thermal properties. PB1413: with UV stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
ASTM D648