Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® P284 PPE Alloy, 10% Glass Reinforced

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 10% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P284 PPE Alloy, 10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 10% glass reinforced PPE Alloy for superior properties and chemical resistance with high heat resistance.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0075 cm/cm
0.0075 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 86.0 MPa
12500 psi
ATSM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Strength 136 MPa
19700 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Vicat Softening Point 239 °C
462 °F
ASTM D1525