Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® P270WO PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Extruded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P270WO PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An extrusion grade for high temperature applications requiring flame retardancy as well as high mechanical strength and toughness such as electrical housings.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Flexural Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 2.51 J/cm
4.70 ft-lb/in
ASTM D256
1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0579 in
UL94