Ashley Polymers Ashlene® P268WO PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Extruded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P268WO PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An extrusion grade for general purpose application requiring flame retardancy and good impact resistance.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ATSM D638
Flexural Strength 57.0 MPa
8270 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
1.50 J/cm

@Temperature -40.0 °C
2.81 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0579 in
UL94