Material Notes:
A general purpose, 20% glass reinforced PPO resin for injection molding applications requiring structural strength, dimensional stability and good heat resistance.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 95.0 MPa
13800 psi
ATSM D638
Flexural Modulus 4.90 GPa
711 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
291 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
ASTM D648