Material Notes:
A flame retardant resin with excellent heat deflection temperature and good impact strength.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ATSM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 2.55 J/cm
4.78 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-1
V-1
V-1 UL94