Material Notes:
A rigid flame retardant polycarbonate, UV stabilized for applications requiring superior dimensional stability and overall toughness. Also available as 1500 without UV stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ATSM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 0.990 J/cm
1.85 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Copyright © lookpolymers.com All Rights Reserved