Ashley Polymers Ashlene® P124WO PBT Polyester, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P124WO PBT Polyester, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant 20% glass reinforced, natural. Colors will modify properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 93.0 MPa
13500 psi
ATSM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 5.40 GPa
783 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
379 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.870 mm
V-0

@Thickness 0.0343 in
Users viewing this material also viewed the following: