Material Notes:
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also available with UV stabilizer, designated D925H.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs; ASTM D570
Water Absorption at Saturation 1.4 %
1.4 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 395 %
395 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
1.10 J/cm

@Temperature -40.0 °C
2.06 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 184 °C
363 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ASTM D648