Material Notes:
General purpose, medium impact resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 1.7 g/10 min
1.7 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ATSM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 2.16 J/cm
4.05 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
192 °F
ASTM D648
Flammability, UL94 HB
HB