Material Notes:
High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Typical value for ABS
Melt Flow 0.70 g/10 min
0.70 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ATSM D638
Flexural Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648