Ashley Polymers Ashlene® 980LS-40G Nylon 612, 40% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 980LS-40G Nylon 612, 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 40% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.14 %
0.14 %
24 hrs; ASTM D570
Water Absorption at Saturation 2.0 %
2.0 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 179 MPa
26000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Modulus 9.70 GPa
1410 ksi
ASTM D790
Izod Impact, Notched 1.34 J/cm
2.51 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 211 °C
412 °F
ASTM D648