Material Notes:
This is an extrusion grade Nylon 6 resin suitable for both coextrusion and blown film applications. It has excellent melt stability and very high melt strength. It also has excellent grease resistance, toughness, resistance to abrasion.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Film Elongation at Break, TD 290 %
290 %
ASTM D882
Secant Modulus, TD 0.650 GPa
94.3 ksi
ASTM D882
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
Film Tensile Strength at Break, TD 60.0 MPa
8700 psi
ASTM D882